logo
products_banner
Position:
Home  >  Products  >  products  >  Pressure vessel steel plate -A517 Grade E
A517 Grade E-145
A517 Grade E-147
A517 Grade E-146
A517 Grade E-148
A517 Grade E-144
A517 Grade E-thumbnail-145
A517 Grade E-thumbnail-147
A517 Grade E-thumbnail-146
A517 Grade E-thumbnail-148
A517 Grade E-thumbnail-144

Pressure vessel steel plate -A517 Grade E

A517 Grade E is an ultra-high-strength low-alloy steel plate that complies with the ASTM A517 standard. It undergoes quenching and tempering heat treatment, achieving a yield strength of ≥1000 MPa while demonstrating excellent impact resistance.

Send Inquiry

Product Description

1.What is the chemical composition of A517 Grade E steel?

A517 grade E Chemical Composition
Grade The Element Max(%)
C Si Mn P S
A517 grade E 0.10-0.22 0.08-0.45 0.35-0.78 0.035 0.035
Cr Mo B Ti
1.34-2.06 0.36-0.64 0.001-0.005 0.005-0.11

 

2.What are the key differences in core parameters between A517 Grade E and A517 Grade Q?

Property A517 Grade E A517 Grade Q
Standard Reference ASTM A517 (Conventional Q&T Steel) ASTM A517 (Cost-Optimized Grade)
Material Type Ni-Cr-Mo Alloy Steel Low-Carbon Microalloyed Steel
Heat Treatment Quenched & Tempered (Q&T) Thermo-Mechanical Controlled Processing (TMCP)
Tensile Strength ≥760 MPa (110 ksi) ≥690 MPa (100 ksi)
Yield Strength ≥690 MPa (100 ksi) ≥620 MPa (90 ksi)
Elongation ≥16% ≥18%
Key Alloying Elements Ni 0.7-1.2%, Cr 0.4-0.8%, Mo 0.2-0.4% Nb 0.02-0.05%, V 0.05-0.10%, Ti ≤0.02%
Impact Toughness -40°C CVN≥54J -20°C CVN≥34J
Welding Preheat Temp. 150-200°C 100-150°C
Max. Thickness ≤150mm ≤100mm
Relative Cost Higher (30-40% more than Grade Q) Lower

 

3.What are the typical applications of A517 Grade E?
• Ultra-high pressure vessels (nuclear/chemical industries)
• Structural components for heavy engineering machinery
• Wear-resistant parts for mining equipment
• Protective components for special equipment

Related Products

Contact GNEE today for more details about Custom-Engineered Solutions.

Sent E-mail